许崇浩, 郑文忠, 胡明亮, 王英. 感应加热破碎型钢混凝土构件试验研究[J]. 工程力学, 2022, 39(4): 100-112. DOI: 10.6052/j.issn.1000-4750.2021.01.0099
引用本文: 许崇浩, 郑文忠, 胡明亮, 王英. 感应加热破碎型钢混凝土构件试验研究[J]. 工程力学, 2022, 39(4): 100-112. DOI: 10.6052/j.issn.1000-4750.2021.01.0099
XU Chong-hao, ZHENG Wen-zhong, HU Ming-liang, WANG Ying. EXPERIMENTAL STUDY ON DEMOLISHING STEEL REINFORCED CONCRETE COMPONENTS BY INDUCTION HEATING[J]. Engineering Mechanics, 2022, 39(4): 100-112. DOI: 10.6052/j.issn.1000-4750.2021.01.0099
Citation: XU Chong-hao, ZHENG Wen-zhong, HU Ming-liang, WANG Ying. EXPERIMENTAL STUDY ON DEMOLISHING STEEL REINFORCED CONCRETE COMPONENTS BY INDUCTION HEATING[J]. Engineering Mechanics, 2022, 39(4): 100-112. DOI: 10.6052/j.issn.1000-4750.2021.01.0099

感应加热破碎型钢混凝土构件试验研究

EXPERIMENTAL STUDY ON DEMOLISHING STEEL REINFORCED CONCRETE COMPONENTS BY INDUCTION HEATING

  • 摘要: 感应加热破碎型钢混凝土(SRC)时,型钢直接被电磁感应加热,混凝土依靠型钢热传导被加热,型钢与混凝土之间产生温度差和变形差,为实现型钢与混凝土之间的分离提供可能。开展了6根无混凝土保护层和8根有混凝土保护层型钢混凝土试件的感应加热分离试验,试验结果表明:不同试件内型钢的温升曲线趋势基本相同,即型钢温度在450 ℃以下时,型钢升温较快,约为30 ℃/min~50 ℃/min;当型钢温度在450 ℃~700 ℃时,型钢温升变慢,约为20 ℃/min~30 ℃/min;当型钢温度达到700 ℃后,型钢温升平缓。当型钢温度不高于700 ℃时,随着型钢温度的升高,型钢与混凝土之间温度差及膨胀差基本呈线性增加。型钢与混凝土的膨胀差主要与型钢腹板高度相关,当型钢腹板高度为300 mm,膨胀差不小于1.80 mm时,可方便型钢与其所辖混凝土的分离;当型钢腹板高度为400 mm,膨胀差不小于2.12 mm时,可方便型钢与其所辖混凝土的分离。

     

    Abstract: In the process of induction heating, the steel is heated directly by electromagnetic induction while the concrete is heated by heat conduction. The temperature and deformation differences between the steel and concrete are produced, which provide the possibility for the separation between the steel and the concrete. The induction heating separation tests of six steel reinforced concrete specimens without protective layers and eight steel reinforced concrete specimens with protective layers were carried out. The test results show that the trend of the temperature rise curve of the steel in different specimens is basically the same. When the temperature of the steel is below 450 ℃, the temperature rise of the steel is fast and the rate is approximately 30 ℃/min ~ 50 ℃/min. When the steel temperature is between 450 ℃ ~ 700 ℃, the steel temperature rise slows down and the rate becomes approximately 20 ℃/min ~ 30 ℃/min. When the steel temperature reaches 700 ℃, the steel temperature rises gently. When the steel temperature is no higher than 700 ℃, the temperature and expansion differences between the steel and the concrete increase linearly. The expansion difference between the section steel and concrete is mainly related to the height of the section steel web. When the height of section steel web is 300 mm and the expansion difference is not less than 1.80 mm, it is convenient to separate the section steel from the concrete. When the height of section steel web is 400 mm and the expansion difference is not less than 2.12 mm, it is also convenient to separate the section steel from the concrete.

     

/